Super garyndy HASTELLOY (r) C276 (UNS N10276) 6.35 * 1,65 mm
Himiki düzümi
Super garyndy HASTELLOY (r) C276 (UNS N10276) 6.35 * 1,65 mm
HASTELLOY (r) C276-nyň himiki düzümi aşakdaky tablisada görkezilýär.
Element | Mazmuny (%) |
---|---|
Nikel, Ni | 57 |
Molibden, Mo. | 15-17 |
Hrom, Cr | 14.5-16.5 |
Demir, Fe | 4-7 |
Volfram, W. | 3-4.50 |
Kobalt, Co. | 2.50 |
Marganes, Mn | 1 |
Wanadim, V. | 0.35 |
Silikon, Si | 0.080 |
Fosfor, P. | 0.025 |
Uglerod, C. | 0.010 |
Kükürt, S. | 0.010 |
Fiziki aýratynlyklar
Super garyndy HASTELLOY (r) C276 (UNS N10276) 6.35 * 1,65 mm
Aşakdaky tablisada HASTELLOY (r) C276-nyň fiziki aýratynlyklary görkezilýär.
Sypatlar | Metrik | Imperial |
---|---|---|
Dykyzlygy | 8,89 g / sm³ | 0.321 fb / in³ |
Ereýän nokat | 1371 ° C. | 2500 ° F. |
Mehaniki aýratynlyklary
Super garyndy HASTELLOY (r) C276 (UNS N10276) 6.35 * 1,65 mm
HASTELLOY (r) C276-nyň mehaniki aýratynlyklary aşakdaky tablisada görkezilýär.
Sypatlar | Metrik | Imperial |
---|---|---|
Dartyş güýji (@ kesel 4.80-25,4 mm, 538 ° C / @ galyňlygy 0,189-1.00, 1000 ° F) | 601.2 MPa | 87200 psi |
Hasyl güýji (0,2% ofset, @ kesel 2,40 mm, 427 ° C / @ galyňlygy 0.0945, 801 ° F) | 204.8 MPa | 29700 psi |
Elastik modul (RT) | 205 GPa | 29700 ksi |
Arakesmede uzalma (50,8 mm, @ kesel 1,60-4.70 mm, 204 ° C / @ galyňlygy 0.0630-0.185, 399 ° F) | 56% | 56% |
Gatylyk, Rokwell B (tabak) | 87 | 87 |
Malylylyk aýratynlyklary
HASTELLOY (r) C276-nyň ýylylyk aýratynlyklary aşakdaky tablisada berilýär.
Sypatlar | Metrik | Imperial |
---|---|---|
Malylylyk giňelmesi bilelikde işleýär (@ 24-93 ° C / 75.2-199 ° F) | 11.2 µm / m ° C. | 6.22 µin / ° F. |
Malylylyk geçirijiligi (-168 ° C) | 7.20 W / mK | 50.0 BTU / sagatda. ° F. |
Beýleki bellikler
HASTELLOY (r) C276-a deň materiallar aşakdaky ýaly.
ASTM B366 | ASTM B574 | ASTM B622 | ASTM F467 | DIN 2.4819 |
ASTM B575 | ASTM B626 | ASTM B619 | ASTM F468 | |