Garyndy 276 Poslamaýan polatdan ýasalan turba turbasynyň bahasy
Hastelloý C276 Himiki düzümi
“SIHE STAINLESS STEEL” halkara standartyna we iň täze täzeliklere görä Harytlary gaplamak üçin tehnologiýada örän döwrebap.Içerki we halkara müşderimize “Premium Hil” önümlerini hödürlemek üçin gaplamaga we belliklere köp üns berýäris.“Hastelloy C276” armaturlary plastik folga we Bubble gatlaklary bilen seresaplylyk bilen gaplanýar we agaç gutulara seresaplylyk bilen ýerleşdirilýär.
Käbir deňeşdirme poslama garşylyk maglumatlary, metbugat, konsentrasiýa we temperaturany öz içine alýan goşmaça ulanyşlary has içgin öwrenmek üçin bize jaň ediň.SIHE STAINLESS STEEL turba we turba ulgamlary barada has giňişleýin maglumat üçin Hastelloy C276 turbamyzy we Hastelloy C276 Tube sahypalaryna serediň.
Hastelloý C276 | Ni | C | Mo | Mn | Si | Fe | P | S | Co | Cr |
| Balans | Iň ýokary 0.010 | 15.00 - 17.00 | Iň ýokary 1.00 | Iň ýokary 0.08 | 4.00 - 7.00 | Iň ýokary 0.04 | Iň ýokary 0.03 | 2,5 maks | 14.50 - 16.50 |
Hastelloý C276 mehaniki aýratynlyklary
Adaty otagyň temperaturasy, dykylan materialyň dartyş aýratynlyklary
Haryt görnüşi | Dartma (ksi) | .2% Hasyl (ksi) | Uzalma% |
Garyndy C276 bar | 110.0 | 52.6 | 62 |
Garyndy C276 plastinka | 107.4 | 50.3 | 67 |
Garyndy C276 sahypasy | 115.5 | 54.6 | 60 |
Garyndy C276 turba we garyndy C276 turba | 105.4 | 45.4 | 70 |
Hastelloý C276 eriş nokady
Fiziki aýratynlyklar | ° F. | Iňlis bölümleri | ° C. | Metrik bölümler |
Dykyzlygy | 72 | 0.321 funt / in.(3) | 22 | 8,89 g / sm (3) |
Eriş aralygy | 2415- | 1323- | ||
Elektrik | 75 | 51 mikrohm. | 24 | 1.30 mikrohm-m |
Orta koeffisiýenti | 75-200 | 6.2 mikroin./in.-°F | 24-93 | 11.2 X 10 (-6) m / mK |
75-400 | 6.7 mikroin./in.-°F | 24-204 | 12.0 X 10 (-6) m / mK | |
75-600 | 7.1 mikroin./in.-°F | 24-316 | 12.8 X 10 (-6) m / mK | |
75-800 | 7.3 mikroin./in.-°F | 24-427 | 13.2 X 10 (-6) m / mK | |
75-1000 | 7.4 mikroin./in.-°F | 24-538 | 13.4 X 10 (-6) m / mK | |
75-1200 | 7.8 mikroin./in.-°F | 24-649 | 14.1 X 10 (-6) m / mK | |
75-1400 | 8.3 mikroin./in.-°F | 24-760 | 14.9 X 10 (-6) m / mK | |
75-1600 | 8.8 mikroin./in.-°F | 24-871 | 15.9 X 10 (-6) m / mK | |
75-1700 | 8.9 mikroin./in.-°F | 24-927 | 16.0 X 10 (-6) m / mK | |
Malylylyk | -270 | 50 Btu-in / ft²-sag- ° F. | -168 | 7.2 W / mK |
-100 | 60 Btu-in / ft²-sag- ° F. | -73 | 8.6 W / mK | |
0 | 65 Btu-in / ft²-sag- ° F. | 32 | 9.4 W / mK | |
100 | 71 Btu-in / ft²-sag- ° F. | 38 | 10.2 W / mK | |
200 | 77 Btu-in / ft²-sag- ° F. | 93 | 11.1 W / mK | |
400 | 90 Btu-in / ft²-sag- ° F. | 204 | 13.0 W / mK | |
600 | 104 Btu-in / ft²-sag- ° F. | 316 | 15.0 W / mK | |
800 | 117 Btu-in / ft²-sag- ° F. | 427 | 16.9 W / mK | |
1000 | 132 Btu-in / ft²-sag- ° F. | 538 | 19.0 W / mK | |
1200 | 145 Btu-in / ft²-sag- ° F. | 649 | 20.9 W / mK | |
1400 | 159 Btu-in / ft²-sag- ° F. | 760 | 22.9 W / mK | |
1600 | 173 Btu-in / ft²-sag- ° F. | 871 | 24.9 W / mK | |
1800 | 185 Btu-in / ft²-sag- ° F. | 982 | 26.7 W / mK | |
2000 | 195 Btu-in / ft²-sag- ° F. | 1093 | 28.1 W / mK |
Hastelloý C276 ekwiwalent
STANDARD | UNS | WERKSTOFF NR. | AFNOR | EN | JIS | BS | GOST |
Hastelloý C276 | N10276 | 2.4819 | - | NiMo16Cr15W | NW 0276 | - | ХН65МВУ |
Haryt aýratynlyklary
ASTM B622, B829 / ASME SB622, SB829 / NACE MR0175
Ölçeg aralygy
Daşarky diametri (OD) | Diwar galyňlygy |
.250 "- 500" | .035 "-. 065" |
Sowuk gutardy we ýagtylandyrylan turba.
Himiki talaplar
Garyndy C276 (UNS N10276)
Kompozisiýa%
Ni Nikel | Cr Hrom | Mo Molibden | Fe Demir | W Volfram | C Uglerod | Si Silikon | Co Kobalt | Mn Marganes | V Wanadim | P Fosforly | S Kükürt |
57.0 min | 14.5–16.5 | 15.0–17.0 | 4.0–7.0 | 3.0–4.5 | Iň ýokary 0.010 | Iň ýokary 0.08 | 2,5 maks | 1.0 max | Iň ýokary 0,35 | Iň ýokary 0.04 | Iň ýokary 0.03 |
Ölçegli çydamlylyk
OD | OD çydamlylygy | Diwar çydamlylygy |
.250 "-. 500" | +.004 ”/ -. 005” | ± 15% |
Mehaniki aýratynlyklary
Hasyl güýji: | 41 ksi min |
Dartyş güýji: | 100 ksi min |
Uzalma (min 2 "): | 40% |